Photo: RudolfSimon, 2012, via Wikimedia Commons (CC BY-SA 3.0)
Every phone, laptop and most electric cars store energy the same way: by sliding lithium ions in and out of two solid hosts. The ions are not used up in a one-way reaction. They shuttle. That is why a lithium-ion cell can be charged hundreds or thousands of times, and why it slowly loses capacity: each trip is a little less reversible than the last.
The 2019 Nobel Prize in Chemistry went to M. Stanley Whittingham, John B. Goodenough and Akira Yoshino for turning that shuttle into a practical battery. This article is about the mechanism they enabled: intercalation, the cathode chemistries that now compete for the same job, what energy density actually measures, why capacity fades, and how a cell can run away thermally. It is not a buying guide. Where sodium-ion, lithium iron phosphate power stations or solid-state packs come in, they are linked rather than retold.
The advantage of lithium-ion batteries is that they are not based upon chemical reactions that break down the electrodes, but upon lithium ions flowing back and forth between the anode and cathode.
That sentence is from the Royal Swedish Academy of Sciences’ 2019 chemistry-prize press release. The rest of this piece is about what those ions are doing, and what goes wrong when the trip is no longer clean.
A shuttle, not a tank
A gasoline tank is a container. A lithium-ion cell is more like two parking structures and a road between them. In solid-state chemistry that parking is called intercalation: guest ions insert into a host crystal without dismantling it. The host expands a little and conducts differently, but it is still the same lattice when the guests leave.
Whittingham, working at Exxon during the 1970s oil shocks, showed that lithium ions could move in and out of layered titanium disulfide. In the Nobel committee’s scientific background, his 1976 cell used a lithium-metal anode and a TiS2 cathode in an organic electrolyte, produced about 2.5 volts, and could be cycled more than a thousand times in the laboratory. The intercalation was reversible. The metallic lithium anode was not. On charge, lithium plated back unevenly and grew dendrites, thin metal whiskers that could pierce the separator, short the cell and start a fire. Exxon’s effort did not become a consumer battery.
The way out was to get rid of the lithium metal. Researchers began building what they called ion-transfer, or "rocking chair," cells: two intercalation hosts, with the lithium already stored as ions inside one of them. On charge, the ions leave the cathode, travel through the electrolyte, and intercalate into the anode. Discharge is the same trip in reverse. Electrons take the external circuit; ions take the electrolyte. Nothing has to plate as a metal, and nothing has to dissolve the electrodes to keep current flowing.
Lithium is a good guest for this job. It is the lightest metal, it forms a small ion, and it has a strongly negative electrochemical potential, so a cell built around it can reach a usefully high voltage. The U.S. Department of Energy’s July 2023 technology strategy assessment on lithium-ion batteries still describes the family in these rocking-chair terms.

Diagram: Sergey WereWolf, 2016, via Wikimedia Commons (CC0 1.0)
The four parts of a cell
A commercial lithium-ion cell has four working parts, plus the metal foils that collect current. The anode in most cells is graphite. In the fully lithiated state it is often written LiC6: one lithium ion for every six carbon atoms in the layered graphite sheets. The cathode is a lithium metal oxide or phosphate; the choice of cathode is the main fork in the chemistry, and we will come back to it. The electrolyte is typically a lithium salt, most often lithium hexafluorophosphate (LiPF6), dissolved in a mixture of organic carbonates. The separator is a thin, porous polymer or ceramic-coated film that lets ions through and keeps the two electrodes from touching.
Those electrodes are coated on current collectors: copper foil on the anode side, aluminum on the cathode side. DOE’s 2023 assessment notes one exception: lithium titanate (LTO) anodes, used when high power or very long cycle life matters more than energy density, also sit on aluminum, because they operate at a potential where copper would be less stable. The coatings also include a conductive carbon additive and a binder that holds the particles on the foil.
A single electrochemical cell is a coated anode, a coated cathode, a separator and electrolyte, rolled or stacked and sealed in a can or pouch. An 18650 cell is about 18 millimeters across and 65 millimeters long. A 21700 cell is a little larger, 21 by 70 millimeters. Pouch and prismatic cells give pack designers flatter shapes. A pack, such as the one in an electric car, is many cells in series and parallel, plus a battery management system, cooling, and the case. DOE’s assessment is blunt about why those extras exist: they extend life, or limit the damage if a cell fails.

Photo: Sevenethics, 2025, via Wikimedia Commons (CC0 1.0)
How a charge cycle moves lithium
Start with a charged cell. Lithium ions are intercalated in the graphite. The cathode is relatively empty of lithium. Connect a load, and electrons leave the anode through the copper foil, travel through the device, and arrive at the cathode. To keep charge balanced, lithium ions unbind from the graphite, cross the electrolyte, and insert into the cathode crystal. The cell voltage falls as the cathode fills and the anode empties. That is discharge.
Charging is the same path backward, forced by a charger. Electrons are pushed into the anode. Ions leave the cathode, cross the electrolyte, and intercalate back into the graphite. The voltage rises. For a typical graphite / layered-oxide cell, the useful window is roughly 3.0 volts at the low end to about 4.2 volts at the high end, with a nominal voltage around 3.6 to 3.7 volts. An LFP cell sits lower, typically around 3.2 to 3.3 volts nominal, because its cathode has a lower potential.
The window is not a suggestion. If the voltage is driven too high, a layered-oxide cathode can shed oxygen and the electrolyte can oxidize. If it is driven too low, the copper collector can dissolve and later plate in places that cause a short. The battery management system exists, in large part, to keep every cell inside that window, and a pack of cells at similar states of charge, so no single cell is pushed over the edge.
The first charge of a new graphite cell is special. Some lithium and some electrolyte are consumed forming a thin film on the anode, the solid electrolyte interphase, or SEI. The Nobel scientific background treats that film as part of what made graphite usable: it passes lithium ions and blocks further solvent breakdown. Without it, the electrolyte would keep reacting with the anode. With it, the cell can cycle. The catch, as we will see, is that the film does not stay frozen in time.
Why the cathode chemistry matters
Once the anode is graphite and the electrolyte is a carbonate solution of LiPF6, most of the design freedom is in the cathode. DOE’s 2023 assessment lists the main commercial classes: lithium cobalt oxide (LCO), lithium nickel manganese cobalt oxide (NMC), lithium nickel cobalt aluminum oxide (NCA), lithium manganese oxide (LMO), and lithium iron phosphate (LFP). They all intercalate lithium. They do not offer the same voltage, energy per kilogram, cycle life, or behavior when they get hot.
Lithium cobalt oxide, the first commercial cell
Goodenough and co-workers at Oxford, in 1979 and 1980, showed that lithium could be extracted from lithium cobalt oxide, LiCoO2, at a much higher voltage than Whittingham’s sulfide. The Nobel press release puts the result at as much as four volts. The 1980 paper, by K. Mizushima, P.C. Jones, P.J. Wiseman and Goodenough, is the layered-oxide starting point for almost every phone battery since.
Yoshino, at Asahi Kasei in 1985, paired a Goodenough-style cobalt oxide cathode with a carbon anode made from petroleum coke, which could intercalate lithium without the dendrites of lithium metal. Lithium-ion cells entered the market in 1991, using that petroleum-coke anode and a lithiated cobalt oxide cathode, as the Nobel scientific background records. Graphite later became the standard anode, once electrolytes were found that built a reliable SEI on it. LCO is still common in phones and laptops, where volume is tight. It is less common in large packs, where cobalt’s cost, supply and safety record are harder to ignore.
NMC and NCA, packing more energy into cars
NMC replaces some of the cobalt with nickel and manganese. The numbers in the name are the ratio: NMC 111 is equal parts nickel, manganese and cobalt; NMC 622 is 60 percent nickel; NMC 811 is 80 percent nickel. More nickel generally means more capacity and less cobalt. It also means a lattice that is less stable when the cell is fully charged, and a greater tendency to release oxygen if the cathode is heated or overcharged. NCA, used for years in some Tesla packs, is a close cousin: nickel and cobalt with aluminum as the stabilizer. In their 2023 MRS Bulletin essay, Whittingham and Jie Xiao noted that Tesla’s high-nickel NCA, written LiNi0.9Co0.05Al0.05O2 in that paper, uses aluminum for that stabilization, and that as nickel content rises, so does the tendency to release gas.
These layered oxides are why a long-range electric car can carry a pack that still fits under the floor. They are also why pack designers worry about cooling, voltage limits and what happens in a crash or a heater failure. The energy is in the voltage and in how much lithium the cathode can reversibly release. The risk is how the structure behaves once a large fraction of that lithium is gone.
Lithium iron phosphate, the heavier, harder-to-ignite cousin
In 1997, A.K. Padhi, K.S. Nanjundaswamy and Goodenough, then at the University of Texas at Austin, reported that lithium iron phosphate, LiFePO4, could serve as a cathode. The material is an olivine, not a layered oxide. In that Journal of the Electrochemical Society paper, the Fe3+/Fe2+ couple sits near 3.5 volts versus lithium metal, lower than the layered oxides, which is why an LFP/graphite cell has a lower nominal voltage and stores less energy per kilogram. The compensation is structural: the phosphate polyanion holds its oxygen more tightly, and the formula contains no cobalt or nickel. The voltage curve is relatively flat, which is slightly annoying for estimating state of charge and useful for making a stable 12-volt-class pack from four cells in series.
LFP is why so many portable power stations now advertise LiFePO4 on the case. The cycle-life claims and the weight penalty in those boxes are covered in our earlier explainer on why so many portable power stations now use LFP. The short version here is that LFP is still a lithium-ion intercalation cell, not a different kind of battery. It is a different host for the same ion, chosen when durability and thermal stability matter more than packing the most watt-hours into the least mass.
What "energy density" actually measures
Energy density is not one number. Gravimetric energy density, in watt-hours per kilogram, tells you how heavy the pack will be. Volumetric energy density, in watt-hours per liter, tells you how large it will be. Both can be quoted at the cell or pack level, and the gap is large, because a pack includes the case, cooling, busbars, fuses and the management electronics.
At the cell level, Whittingham and Xiao wrote in 2023 that today’s commercial lithium-ion cells attain around 250 Wh/kg and 700 Wh/L, up sharply from two decades earlier, while large-quantity costs had fallen from around $5,000 per kilowatt-hour to around $100. Those are commercial cell figures, not laboratory records, and not pack figures. The U.S. Department of Energy’s Vehicle Technologies Office, in its 2023 batteries overview, set a near-term research target of 300 Wh/kg for improved graphite/NMC cells, 400 Wh/kg for next-generation cells that bring in substantial silicon at the anode, and 500 Wh/kg as a longer-term goal for lithium-metal cells, the Battery500 class of work.
Pack numbers are lower. Argonne National Laboratory’s BatPaC 5.2 model, used in the laboratory’s November 2024 GREET battery update, puts a 300-mile electric car pack at about 143 Wh/kg with an LFP cathode and about 198 Wh/kg with NMC 811. A still-higher-nickel "NMC 95" pack in the same table reaches about 205 Wh/kg. Those are all-in pack estimates for a specific vehicle class and range, not a promise about any one manufacturer’s module. They are useful because they compare chemistries on the same basis, inactive mass included.
The pattern is consistent. Layered nickel-rich oxides win on watt-hours per kilogram. LFP wins on what that table does not show as clearly: cycle life under clumsy use, freedom from nickel and cobalt, and a milder response if the cell is abused. Phones stay with LCO or similar dense oxides because a few extra watt-hours in a few millimeters matter more than surviving thousands of cycles. Grid cabinets, many buses and many standard-range cars have moved the other way.
As an Amazon Associate, Aglena earns from qualifying purchases.
Why lithium-ion cells lose capacity
If intercalation does not destroy the electrodes, why does a five-year-old phone hold less charge than it did on day one? Because the shuttle is only almost reversible. The standard review is still J. Vetter and colleagues’ 2005 paper in the Journal of Power Sources, "Ageing mechanisms in lithium-ion batteries," which separates the damage into a few recurring modes rather than a single wear-out.

Photo: Retired electrician, 2026, via Wikimedia Commons (CC0 1.0)
The first is loss of cyclable lithium. The SEI on the graphite anode grows and repairs itself over time, especially at high temperature and at a high state of charge. Every increment of new film consumes lithium ions and electrolyte that will not return to the cathode on the next discharge. The hosts may still be there, but there are fewer shuttling ions to fill them. That is why a cell can lose capacity on the shelf: calendar aging is real, and it is faster when the cell is stored full and warm.
The second is loss of active material. Cathode particles crack as they swell and shrink. Transition-metal ions, especially from some layered oxides, can dissolve into the electrolyte and migrate to the anode. Graphite can exfoliate if the SEI is clumsy or if solvent co-intercalates. Silicon, added to raise anode capacity, undergoes much larger volume changes than graphite and can lose electrical contact with the foil. In all of these cases, parts of the electrode stop participating even if lithium remains.
The third, and the one that can also become a safety problem, is lithium plating. If you charge too fast, or at low temperature, the anode may not accept ions into the graphite fast enough. The surface potential drops until metallic lithium begins to plate on the anode instead of intercalating. Some of that metal becomes isolated and is lost to the shuttle. Some of it can grow dendrites, the same class of hazard that stopped Whittingham’s lithium-metal cell from becoming a consumer product. That is why manufacturers derate fast charging in the cold, and why a management system may refuse a charge until the pack is warm enough.
How hard you cycle the cell matters, but so does how you leave it. High state of charge holds the cathode in a more oxidized, more reactive state and thickens the SEI. High temperature accelerates almost every parasitic reaction. Warranties therefore pick a convention, often 80 percent of original capacity after a stated number of cycles under stated conditions. DOE’s 2023 assessment, writing about stationary systems, says lithium-ion batteries often have a life or warrantied life of 10-plus years and 1,000-plus cycles, and that how the battery is used and controlled can dramatically change that life. LFP cells are routinely rated for several thousand cycles to a similar retention; layered-oxide cells used for maximum range are often rated more conservatively, though a tight SOC window can stretch their calendar life as well. The number on a spec sheet is a test condition, not a law of nature.
Thermal runaway, and why chemistry still matters when a cell gets hot
Thermal runaway is a self-heating cascade that a cell cannot reject to its surroundings fast enough to stop. It is not the same thing as ordinary fade, but the same chemistry sits underneath. A common sequence, seen in accelerating-rate calorimetry at national laboratories, starts with breakdown of the SEI at elevated temperature, which exposes lithiated graphite to the electrolyte and generates more heat. The electrolyte decomposes. The separator can shrink or melt and allow an internal short. In layered-oxide cells, the delithiated cathode can then release oxygen, which feeds combustion of the organic electrolyte. Once that loop is closed, the heating rate can jump by orders of magnitude.
The cathode chemistry changes the violence of that loop more than it changes the first whisper of heat. A U.S. Department of Energy abuse-tolerance study using accelerating-rate calorimetry on 18650 cells, reported in the Vehicle Technologies Office’s progress documentation, measured peak heating rates on the order of 175 to 225°C per minute for NMC/graphite cells, and about 1.5°C per minute for LFP/graphite cells under the conditions of that test. The LFP cell was not inert, but its cathode did not pour oxygen into the reaction the way the layered oxides did. A later open-access study of commercial 21700 cells in the journal Batteries likewise found that LFP cells went into runaway later and at higher temperatures than NMC and NCA cells, and that at low states of charge some cells did not run away at all up to the 350°C stop of the test.
Those figures are laboratory results on specific cells, not a guarantee about a module in a car or a storage cabinet. State of charge, cell size, whether the pack can vent, and whether one failed cell can heat its neighbors all change the outcome. LFP is meaningfully harder to drive into a violent runaway. It is not incapable of failing, and a pack still needs a management system, mechanical protection and a plan for a short, a crush or external heat. Cell-level tests such as UL 1642 and IEC 62133, and system-level work such as UL 9540A for stationary storage, exist because the chemistry is energetic enough to need them.
What sits outside this chemistry
The intercalation idea is not limited to lithium. Sodium-ion batteries use a larger, heavier, much more abundant ion in a similar rocking-chair design. They trade energy density for cost and materials security, which is why they are being bought first for stationary storage rather than for phones. Sodium-ion is a cousin, not a rebuttal, of the lithium-ion mechanism.
Replacing the flammable liquid electrolyte is the bet behind solid-state batteries. A solid ion conductor could, in principle, enable a lithium-metal anode and cut some of the thermal-runaway pathways that start in the liquid. The manufacturing problems that have kept that idea in test cars are a separate article. So is long-duration storage that leaves intercalation behind, including 100-hour iron-air batteries, which store energy by rusting and un-rusting iron rather than by shuttling ions in and out of a crystal.
Those alternatives exist because lithium-ion has a particular shape. It is excellent at packing reversible energy into a portable box and cycling that box daily for years. It is less natural at holding energy for a week, ignoring nickel and lithium supply, or being indifferent to heat. The intercalation cell is not about to vanish. The point is to know what it is good at, and why a five-year-old pack is never quite the same.
The bottom line
A lithium-ion battery stores energy by intercalating lithium ions in one solid host and taking them back out of another. Whittingham showed that the insertion chemistry works. Goodenough pushed the cathode voltage up with layered oxides, and later with an olivine phosphate. Yoshino removed the metallic lithium anode and made a cell that could be sold. Everything since has been a choice of hosts, electrolytes and packaging around that same rocking chair.
Choose a nickel-rich NMC or NCA cathode and you get more watt-hours per kilogram, which is why long-range cars still rely on them, and you inherit a more reactive charged state. Choose LFP and you give up some of that density for a cathode that is more reluctant to release oxygen, lasts more cycles under hard use, and does not need nickel or cobalt. In either case, capacity fades because the SEI slowly consumes cyclable lithium, because particles crack and lose contact, and because fast or cold charging can plate lithium metal where intercalation was supposed to occur. Thermal runaway is the same chemistry with the heat balance lost.
The ions still flow back and forth, a little less perfectly every year. That is not a flaw in the idea. It is what a real intercalation cell does when films grow, lattices strain and a charger asks more than the anode can take.
Further reading

Bottled Lightning: Superbatteries, Electric Cars, and the New Lithium Economy
Seth Fletcher’s history of the rechargeable lithium-ion cell, from laboratory intercalation chemistry to the electric-car and materials race that followed.

The Powerhouse: America, China, and the Great Battery War
Steve LeVine’s account of the Argonne-linked effort to build a better lithium-ion cathode, and of how that laboratory race became an industrial one.

Volt Rush: The Winners and Losers in the Race to Go Green
Henry Sanderson on the lithium, nickel and cobalt supply chains that sit behind every intercalation cell, and on who wins and loses as those metals are mined.

Material World: The Six Raw Materials That Shape Modern Civilization
Ed Conway’s tour of the materials that underpin modern life, including the lithium and copper that lithium-ion packs cannot do without.

Lithium-Ion Batteries: Basics and Applications